California Bearing Ratio Test Guide

Run laboratory CBR testing under ASTM D1883-21 and AASHTO T 193, apply zero correction, calculate 0.1-in. and 0.2-in. ratios, and verify subgrade CBR.

Laboratory California Bearing Ratio load frame with a cylindrical steel mold, stacked annular surcharge weights, penetration piston, proving ring, and dial gauges
Laboratory CBR loading frame setup with annular surcharge weights, proving ring, and penetration dial gauge.

The California Bearing Ratio (CBR) test under ASTM D1883-21 and AASHTO T 193 measures soil penetration resistance by driving a standardized piston into compacted soil and dividing that load by the standard load for well-graded crushed stone at 2.54 mm (0.1 in.) or 5.08 mm (0.2 in.) penetration, expressed as a percentage.

A high-quality well-graded crushed stone serves as the reference benchmark with a CBR of 100%. Evaluating specimens after soaking and correcting any concave-upward seating tail on the load-penetration curve prevents engineers from overstating the bearing capacity of fine-grained pavement subgrades.

What is the California Bearing Ratio test used for in pavement design?

In pavement design, the California Bearing Ratio test evaluates the potential strength of subgrade, subbase, and base course materials—including recycled materials—for flexible roads and airfield pavements. Originally developed by the California Division of Highways around 1930 and adopted by ASTM as ASTM D 1883 in 1961, CBR serves as an empirical index rather than a fundamental elastic modulus.

Although mechanistic and mechanistic-empirical pavement design methods cannot use CBR directly as a fundamental stiffness property, transportation agencies continue to specify it because the test is straightforward, has an extensive empirical history, and correlates reasonably well with resilient modulus. Laboratory testing follows ASTM D1883-21 or AASHTO T 193, while in-place field testing follows ASTM D 4429 using a similar penetration procedure.

Field CBR measurements under ASTM D 4429 require anchoring the deflection dial well outside the loaded area. Because field testing measures soil at its existing in-situ moisture content whereas laboratory tests normally evaluate soaked specimens, soil-specific correlations are often required to compare field and laboratory CBR values.

CBR sits in the middle of the earthwork testing sequence within sitework, earthmoving, and drainage. Target specimen dry unit weights come from Proctor compaction testing (ASTM D698 or D1557), while daily embankment and lift density verification during construction relies on nuclear density gauge testing.

How is the laboratory CBR test procedure performed step by step?

The laboratory CBR procedure prepares three identically compacted soil specimens at the specified moisture content and dry unit weight, places annular surcharge weights over a perforated swell plate, soaks the assembly for 96 hours while tracking swell, and drives a 50 mm (1.969 in.) piston at 1.25 to 1.3 mm/min (0.05 in./min) while recording penetration loads.

Specimen preparation and compaction

ASTM D1883-21 is primarily intended for materials with a maximum particle size less than 19 mm (0.75 inches). When a sample contains particles larger than 19 mm, the standard modifies the gradation so all tested soil passes the 19-mm sieve while keeping the total gravel fraction—material passing the 3-in. (75-mm) sieve and retained on the No. 4 (4.75-mm) sieve—unchanged. Materials with substantial material retained on the No. 4 (4.75 mm) sieve produce more variable CBR results than finer materials and may require additional trials to establish a reliable design value.

Dry unit weight targets are usually given as a percentage of maximum dry unit weight determined by ASTM D698 or D1557, and each CBR test series uses three identically compacted specimens for a given relative compaction and moisture content. Self-cementing materials that gain strength over time must be cured as directed by the client based on a geotechnical engineering evaluation before penetration testing.

In a standard cylindrical mold measuring 150 mm inside diameter by 175 mm height—equipped with a 50 mm detachable extension collar and a 10 mm thick perforated base plate—dynamic compaction uses either light effort (3 equal layers, 55 blows per layer with a 2.6 kg rammer) or heavy effort (5 layers, 56 blows per layer with a 4.89 kg rammer).

Soaking period and surcharge loading

Unless the requesting client specifies otherwise or soaking has been shown to have no effect on the tested soil, all laboratory CBR specimens must be soaked prior to penetration to represent severe long-term moisture conditions. Annular metal surcharge weights of 2.5 kg each—each representing roughly 7 cm of overlying construction—are stacked on top of the specimen to replicate the confining weight of the planned base and pavement layers, with a minimum of two weights required.

The mold assembly and surcharge weights are immersed in a water tank and soaked for 96 hours (four days). Throughout this four-day soaking period, vertical swelling and water absorption are measured with dial gauges.

Two compacted soil specimens in steel cylindrical CBR molds submerged in a laboratory soaking tank with perforated swell plates, annular surcharge weights, and tripod-mounted dial gauges
Submerged CBR molds fitted with perforated swell plates, annular surcharge weights, and tripod dial gauges to monitor vertical expansion during the 96-hour soak.

Piston penetration and post-test moisture sampling

After soaking, the mold assembly and surcharge weights are transferred to a compression loading machine rated for at least 5,000 kg capacity. The technician seats the 50 mm (1.969 in.) diameter metal penetration piston at the center of the specimen using the smallest possible load—never exceeding 4 kg—to establish full contact before zeroing the load and penetration dials.

The loading frame drives the piston into the specimen at a uniform rate of 1.25 to 1.3 mm/min (0.05 in./min). Total load is recorded across penetration increments from 0.64 mm (0.025 in.) up to 7.62 mm (0.300 in.), with standard evaluations centered at 0.1 in. and 0.2 in. and optional readings extending to 0.3, 0.4, and 0.5 inches. Once loading concludes, 20 to 50 g of soil is collected from the top 3 cm layer to measure post-test moisture content.

Procedural stageStandard parameter or toleranceEngineering purpose
Gradation screeningMaximum particle size under 19 mm (0.75 in.); preserve 3-in. (75-mm) to No. 4 (4.75-mm) gravel fractionPrevents large aggregate from skewing piston resistance in the mold
Mold and compaction150 mm diameter by 175 mm height mold; 3 layers x 55 blows (2.6 kg) or 5 layers x 56 blows (4.89 kg); three specimensMatches laboratory target density from ASTM D698 or D1557
Surcharge and soakingMinimum two 2.5 kg annular weights (7 cm equivalent each); 96 hours (four days) immersionSimulates pavement overburden confinement and long-term moisture weakening
Piston seating and rate50 mm (1.969 in.) piston; seating load at most 4 kg; rate 1.25 to 1.3 mm/min (0.05 in./min)Maintains uniform plastic shear loading on a machine rated at least 5,000 kg
Post-test moisture20 to 50 g sampled from the top 3 cm layerDocuments surface moisture condition directly in the penetration zone

How do you calculate the California Bearing Ratio from piston load?

Calculate the California Bearing Ratio by dividing the corrected unit pressure (or load) required to push the piston to 2.54 mm (0.1 in.) or 5.08 mm (0.2 in.) penetration by the standard reference pressure for well-graded crushed stone at the same depth, then multiplying by 100.

In plain formula form using consistent units:

CBR (%) = (Corrected unit load on specimen / Standard crushed-stone unit load) x 100

At 2.54 mm (0.1 in.) penetration, the standard unit pressure for well-graded crushed stone is 1,000 psi (6.9 MPa). At 5.08 mm (0.2 in.) penetration, the standard unit pressure is 1,500 psi (10.3 MPa). When working directly in force units for the 50 mm diameter piston, the standard crushed-stone loads are 1,370 kgf (13.44 kN) at 2.5 mm penetration and 2,055 kgf (20.15 kN) at 5.0 mm penetration.

Penetration depthStandard unit pressure (US customary / SI)Standard total load (metric force)Design role
2.5 mm / 2.54 mm (0.1 in.)1,000 psi (6.9 MPa)1,370 kgf (13.44 kN)Primary governing penetration depth
5.0 mm / 5.08 mm (0.2 in.)1,500 psi (10.3 MPa)2,055 kgf (20.15 kN)Secondary check depth; requires retest if higher
7.5 mm (0.3 in.)Not primary design reference2,630 kgOptional extended curve tracking
10.0 mm (0.4 in.)Not primary design reference3,180 kgOptional extended curve tracking
12.5 mm (0.5 in.)Not primary design reference3,600 kgOptional extended curve tracking

All observed and calculated values under ASTM D1883-21 shall conform to Practice D6026 guidelines for significant digits and rounding. Because high-quality crushed stone represents 100% CBR, a granular base material performing near standard crushed stone—such as the AASHO Road Test granular base near CBR 100—produces corrected stresses close to 1,000 psi at 0.1 in. and 1,500 psi at 0.2 in., whereas weaker granular subbase around CBR 30 develops proportionally lower bearing resistance.

How do engineers interpret CBR test curves and results?

Engineers interpret CBR test results by first checking the stress-penetration plot for an initial concave-upward curve that requires a tangent zero-point shift, then verifying whether the 2.5 mm ratio exceeds the 5 mm ratio, and finally confirming that moisture conditions match any downstream resilient modulus correlation.

Applying zero-point correction on concave-upward curves

Surface irregularities or incomplete initial piston seating often produce a stress-penetration curve whose early portion is concave upward rather than rising smoothly from zero. When the initial portion of the curve is concave upward, apply a zero correction by drawing a straight tangent line along the curve at the point of greatest slope and extending it downward to intersect the horizontal penetration axis.

That intersection point establishes the shifted origin. Measure the 0.1 in. (2.5 mm) and 0.2 in. (5.0 mm) penetration distances from the corrected origin—not from the raw machine zero—and read the corresponding corrected load values before computing the CBR percentage. Skipping this zero shift artificially depresses or distorts the 0.1-in. bearing ratio.

CBR penetration stress versus penetration graph showing a concave-upward initial tail, a dashed tangent line intersecting the horizontal axis at the corrected origin, and vertical guide lines at +0.10 in. and +0.20 in.
Zero-point correction for an initially concave-upward CBR stress-penetration curve: project a tangent from the steepest slope to set the corrected origin before reading +0.10 in. and +0.20 in. stresses.

Checking 5 mm versus 2.5 mm bearing ratios

In most compacted soils, the calculated CBR at 2.5 mm (0.1 in.) penetration is higher than the ratio at 5 mm (0.2 in.) penetration, and the 2.5 mm value governs design. If the calculated CBR at 5 mm exceeds the CBR at 2.5 mm, the test should be repeated. Only when the repeat test confirms identical behavior should the engineer adopt the 5 mm CBR value for design.

Soaked versus as-compacted behavior and resilient modulus correlations

Laboratory reporting must always state specimen compaction density and soaking status clearly. According to the FHWA Geotechnical Aspects of Pavements Reference Manual (Chapter 5.4), CBR values measured on as-compacted specimens at optimum moisture and density can be significantly higher than CBR values measured on similar specimens after soaking.

In fine-grained silts and clays compacted dry of optimum moisture content, subsequent saturation can cause a steep loss in CBR strength—dropping even below the strength of the same soil compacted wet of optimum—while also generating greater swelling because dry clays absorb more water, as documented in FHWA Chapter 7 on subgrade compaction. By contrast, large wetting-induced strength losses are far less pronounced or negligible in coarse-grained soils.

When converting CBR into resilient modulus (MR) for mechanistic-empirical pavement design or estimating in-situ CBR from field dynamic cone penetrometer (DCP) data, correlations must match moisture and density states. NCHRP 1-37A strongly recommends against using the older 1993 AASHTO Heukelom and Klomp (1962) linear equation and instead provides a nonlinear power correlation.

Correlation purposePublished equationApplicability and engineering note
NCHRP 1-37A resilient modulus (US customary)MR (psi) = 2555 x (CBR)^0.64Preferred NCHRP 1-37A correlation; match soaked or optimum moisture state
NCHRP 1-37A resilient modulus (SI)MR (MPa) = 17.6 x (CBR)^0.64Metric equivalent of the NCHRP 1-37A power relationship
1993 AASHTO / Heukelom and Klomp (1962)MR (psi) = 1500 x CBRLegacy relation for CBR at or below 10; NCHRP 1-37A recommends against use
Dynamic Cone Penetrometer (ASTM D6951)CBR = 292 / (DCP^1.12)Estimates in-situ CBR from penetration index in shallow pavement layers

What is the normal range of CBR values across coarse and fine soils?

Typical field CBR values span from 60 to 80 in well-graded gravel (GW) and 20 to 40 in well-graded sand (SW) down to 5 to 15 in low-plasticity silt (ML) and lean clay (CL), reaching 3 to 5 in fat clay (CH) and organic clay (OH).

The table below summarizes typical field CBR ranges by Unified Soil Classification System (USCS) group from FHWA Table 5-28.

Soil groupUSCS symbolTypical field CBR range
Well-graded gravelGW60 to 80
Poorly graded gravelGP35 to 60
Silty gravelGM40 to 80
Clayey gravelGC20 to 40
Well-graded sandSW20 to 40
Poorly graded sandSP15 to 25
Silty sandSM20 to 40
Clayey sandSC10 to 20
Low-plasticity siltML5 to 15
Lean clayCL5 to 15
Organic siltOL4 to 8
Elastic siltMH4 to 8
Fat clayCH3 to 5
Organic clayOH3 to 5

For quick subgrade and subbase screening, the Iowa State University SUDAS Design Manual (Section 6E-1) organizes CBR values into relative engineering ratings. Generally, clays register CBR values of 6 or less, silty and sandy soils fall around 6 to 8, and road-building sands and gravels normally exceed 10. In the AASHO Road Test, granular base material tested near CBR 100 and granular subbase near CBR 30.

CBR rangePavement layer roleRelative support rating (Iowa SUDAS)
Above 80SubbaseExcellent
50 to 80SubbaseVery Good
30 to 50SubbaseGood
20 to 30SubgradeVery good
10 to 20SubgradeFair-good
5 to 10SubgradePoor-fair
Below 5SubgradeVery poor

What determines the minimum CBR value needed for a road subgrade?

Subgrade design guidance in the Iowa SUDAS manual targets a minimum CBR of 10 because subbase layers placed over subgrades below CBR 10 deflect along with the subgrade under traffic loads, accelerating distress in flexible pavements and eventually rigid pavements. Required thickness increases nonlinearly as subgrade CBR drops below 10.

Because the thickness relationship is nonlinear, a one-unit drop from CBR 5 to 4 demands a larger increase in pavement thickness than a one-unit drop from CBR 10 to 9. In FHWA Table 7-11, subgrades with CBR below 3 (resilient modulus below 30 MPa) are classified as soft, whereas subgrades with CBR from 3 to 8 (resilient modulus from 30 to 80 MPa) are classified as firm to very stiff. FHWA does not recommend placing base or subbase thicknesses less than 150 mm (6 in.) over soft subgrade.

Achieving the design CBR in the field requires tying laboratory testing directly to lift moisture and compaction control. Iowa SUDAS specifies compacting cohesive pavement subgrades to 95% of Standard Proctor at a moisture content between optimum and 4% above optimum, compacting cohesionless sands and gravels to at least 65% relative density, and placing thick layers in lifts of 6 to 8 inches.

Laboratory submittal and curve-correction review checklist

Before accepting a CBR laboratory report into pavement thickness design or subgrade approval, verify every item in the review matrix below.

Review itemRequired documentationVerification trigger
Test standard and gradationASTM D1883-21 or AASHTO T 193; maximum particle size under 19 mm or documented gravel-fraction modificationFlag high variability if substantial particles are retained on the No. 4 (4.75 mm) sieve
Compaction referenceASTM D698 or D1557 target dry unit weight, molding moisture, and three-specimen setVerify borrow-source consistency with the project Proctor report
Soaking and swell record96-hour (four-day) immersion, minimum two 2.5 kg surcharge weights, swell and water absorption readingsConfirm soaked condition unless written geotechnical exemption applies
Load-penetration curvePenetration rate 1.25 to 1.3 mm/min (0.05 in./min), seating load at most 4 kg, raw plotApply steepest-slope tangent zero correction if the initial curve is concave upward
Governing ratio checkCorrected CBR at 2.5 mm (0.1 in.) and 5.0 mm (0.2 in.) rounded per Practice D6026Require repeat test whenever 5.0 mm CBR exceeds 2.5 mm CBR
Post-test moisture and design transferTop 3 cm moisture sample (20 to 50 g); matched moisture state for MR correlationUse NCHRP 1-37A power relation instead of legacy 1500 x CBR equation

Frequently asked questions

Why must laboratory CBR specimens be soaked for 96 hours before penetration?

Under ASTM D1883-21, all specimens must be soaked prior to penetration unless the requesting client specifies otherwise or testing confirms soaking does not affect the soil. Soaking for 96 hours (four days) simulates severe long-term field moisture conditions and exposes sharp strength loss and swelling in fine-grained clays and silts that appear artificially strong when compacted dry of optimum.

What should be done if the CBR at 5 mm (0.2 in.) is higher than at 2.5 mm (0.1 in.)?

Normally the CBR at 2.5 mm (0.1 in.) penetration exceeds the value at 5 mm (0.2 in.) and governs design. If the 5 mm CBR exceeds the 2.5 mm CBR, the laboratory should repeat the test; only if the check test produces identical results should the 5 mm CBR value be adopted for pavement design.

How does the zero-point correction work on a concave-upward CBR curve?

When the early portion of the load-penetration curve bends concave upward due to surface seating effects, draw a straight tangent along the curve at its steepest slope and extend it downward to the horizontal penetration axis. Treat that intercept as the corrected zero origin and measure the 0.1-in. (2.5 mm) and 0.2-in. (5.0 mm) penetrations from that shifted point.

Can a CBR value exceed 100%?

Well-graded crushed stone establishes the 100% reference benchmark at standard loads of 1,000 psi (6.9 MPa) for 0.1 in. penetration and 1,500 psi (10.3 MPa) for 0.2 in. penetration. Materials stiffer than the reference crushed stone—or high-density granular bases near the AASHO Road Test base benchmark of 100—can reach or exceed 100%, while typical field gravels span 35 to 80 and clays generally have CBR values of 6 or less.

How do field CBR and Dynamic Cone Penetrometer tests compare to laboratory CBR?

Field in-place CBR testing follows ASTM D 4429 at existing field moisture with the deflection dial anchored well outside the loaded area, so soil-specific correlations are often required to match soaked laboratory CBR values. For rapid shallow pavement checks, Dynamic Cone Penetrometer testing under ASTM D6951 estimates in-situ CBR using 292 divided by DCP raised to the 1.12 power.

Sources

Related Engineering Guides

Continue with a related construction question.

Explore the topic →